Abstract
This chapter focuses on the sustainability metrics of advanced high-strength steels. It presents a discussion on CO2 emissions and energy intensity. The chapter provides an overview on the life-cycle assessment. It also discusses the economics of advanced high-strength steels.
You do not currently have access to this chapter.
Citation
Sustainability and Economics of Advanced High-Strength Steels, Advanced High-Strength Steels: Science, Technology, and Applications, Second Edition, By Mahmoud Y. Demeri, ASM International, 2024, p 275–292, https://doi.org/10.31399/asm.tb.ahsssta2.t59410275
Download citation file:
Related Book Content
Advanced Steels for Forming Operations
Metallography of Steels Interpretation of Structure and the Effects of Processing
Applications of Advanced High-Strength Steels
Advanced High-Strength Steels: Science, Technology, and Applications, Second Edition
Global Projects on Advanced High-Strength Steels
Advanced High-Strength Steels: Science, Technology, and Applications, Second Edition
Evolving Grades of Advanced High-Strength Steels
Advanced High-Strength Steels: Science, Technology, and Applications, Second Edition
Integrated Computational Materials Engineering Approach to Advanced High-Strength Steels Development
Advanced High-Strength Steels: Science, Technology, and Applications, Second Edition
Introduction to Advanced High-Strength Steels
Advanced High-Strength Steels: Science, Technology, and Applications, Second Edition
Design Guidelines for Advanced High-Strength Steels
Advanced High-Strength Steels: Science, Technology, and Applications, Second Edition
Advanced High-Strength Steels
Advanced High-Strength Steels: Science, Technology, and Applications, Second Edition
Nanosteels
Advanced High-Strength Steels: Science, Technology, and Applications, Second Edition
Forming of Advanced High-Strength Steels (AHSS)
Sheet Metal Forming Processes and Applications