Abstract
This chapter presents the composition, microstructure, processing, deformation mechanism, mechanical properties, formability, and attributes of transformation-induced plasticity steels.
You do not currently have access to this chapter.
Citation
Transformation-Induced Plasticity Steels, Advanced High-Strength Steels: Science, Technology, and Applications, Second Edition, By Mahmoud Y. Demeri, ASM International, 2024, p 127–137, https://doi.org/10.31399/asm.tb.ahsssta2.t59410127
Download citation file:
Related Book Content
Complex-Phase Steels
Advanced High-Strength Steels: Science, Technology, and Applications, Second Edition
Austenitic Stainless Steels
Advanced High-Strength Steels: Science, Technology, and Applications, Second Edition
Twinning-Induced Plasticity Steels
Advanced High-Strength Steels: Science, Technology, and Applications, Second Edition
Martensitic Steels
Advanced High-Strength Steels: Science, Technology, and Applications, Second Edition
Dual-Phase Steels
Advanced High-Strength Steels: Science, Technology, and Applications, Second Edition
Dual-Phase Steels
Advanced-High Strength Steels Science, Technology, and Applications
Complex-Phase Steels
Advanced-High Strength Steels Science, Technology, and Applications
Twinning-Induced Plasticity Steels
Advanced-High Strength Steels Science, Technology, and Applications
Austenitic Stainless Steels
Advanced-High Strength Steels Science, Technology, and Applications
Low-Carbon Steels
Steels: Processing, Structure, and Performance (Second Edition)