Skip Nav Destination
ASM Technical Books
Powder Metallurgy and Additive Manufacturing: Fundamentals and AdvancementsAvailable to Purchase
ASM International
ISBN electronic:
978-1-62708-479-6
Publication date:
2024
Book Chapter
Chapter 15: Role of Powder Metallurgy Industries in Various Sectors―Part 2 Available to Purchase
By
Gulfem Binal
;
Gulfem Binal
Bartin University
, Bartin, Turkey
Search for other works by this author on:
Dervis Ozkan
;
Dervis Ozkan
Bartin University
, Bartin, Turkey
Search for other works by this author on:
Yasin Ozgurluk
;
Yasin Ozgurluk
Bartin University
, Bartin, Turkey
Search for other works by this author on:
Sefa Erdem Yilmaz
;
Sefa Erdem Yilmaz
Bartin University
, Bartin, Turkey
Search for other works by this author on:
Abdullah Cahit Karaoglanli
Abdullah Cahit Karaoglanli
Bartin University
, Bartin, Turkey
Search for other works by this author on:
-
Published:2024
Page range:
337 - 366
Abstract
This chapter explains how powder metallurgy technologies are being leveraged for the production of automotive components, electric motors, rare-earth permanent magnets, and the infrastructure for high-speed rail transport.
You do not currently have access to this chapter.
Citation
Gulfem Binal, Dervis Ozkan, Yasin Ozgurluk, Sefa Erdem Yilmaz, Abdullah Cahit Karaoglanli, Role of Powder Metallurgy Industries in Various Sectors―Part 2, Powder Metallurgy and Additive Manufacturing: Fundamentals and Advancements, Edited By Shashanka Rajendrachari, Debasis Chaira, ASM International, 2024, p 337–366, https://doi.org/10.31399/asm.tb.pmamfa.t59400337
Download citation file:
Related Book Content
Evolution of Powder Metallurgy
Powder Metallurgy and Additive Manufacturing: Fundamentals and Advancements
Appendix
Powder Metallurgy and Additive Manufacturing: Fundamentals and Advancements
Powder Metallurgy
Metals Fabrication Understanding the Basics
Dedication
Powder Metallurgy and Additive Manufacturing: Fundamentals and Advancements
Preface
Powder Metallurgy and Additive Manufacturing: Fundamentals and Advancements
About the Editors
Powder Metallurgy and Additive Manufacturing: Fundamentals and Advancements
Effect of Strain Rate on the Failure Mode of a Rear Axle
Handbook of Case Histories in Failure Analysis
Plastics
Gear Materials, Properties, and Manufacture
Automotive and Transportation Applications
Stainless Steels for Design Engineers