This chapter provides a qualitative overview of powder preparation technologies including milling, mechanical alloying, electrolytic dissolution, metal oxide reduction, solid-state reactive synthesis, and gas, water, and centrifugal atomization. It discusses the general implementation of each process, the materials for which they are used, and the powder characteristics that can be achieved.