Chapter 5: Surface Hardening of Steel
-
Published:2024
Page range:
85 - 119
Abstract
This chapter describes case depth and discusses flame hardening, laser heat treatment, electron beam hardening, induction heat treatment, and induction hardening.
You do not currently have access to this chapter.
Citation
Surface Hardening of Steel, Practical Heat Treating: Processes and Practices, By Jon L. Dossett, ASM International, 2024, p 85–119, https://doi.org/10.31399/asm.tb.phtpp.t59380085
Download citation file:
Related Book Content
Flame and Induction Hardening
Practical Heat Treating (Second Edition)
Selecting Steels for Case Hardening
Heat Treating of Irons and Steels
Localized Heat Treating
Metals Handbook Desk Edition (2nd Edition)
Standards and Inspection
Practical Induction Heat Treating (Second Edition)
Induction Case Hardening of Axle Shafts
Induction Heating and Heat Treatment
Defects and Abnormal Characteristics of Induction Hardened Components
Induction Heating and Heat Treatment
Surface Hardening
Steels: Processing, Structure, and Performance (Second Edition)
Inspection and NDT Methods
Induction Heating and Heat Treatment
Principles of Induction Hardening and Inspection
Induction Heating and Heat Treatment
Austenitizing and Typical Heat Treatment Temperatures for Steels
Heat Treating of Irons and Steels