Abstract
This chapter discusses furnace atmospheres. It describes how furnace atmospheres protect metals, transfer heat, and supply alloying elements (carbon and nitrogen). The chapter focuses on the different types of atmospheres that are available to the heat treater: combustion products, air, exothermic, salt, nitrogen, endothermic, ammonia, hydrogen, inert gas, and vacuum.
You do not currently have access to this chapter.
Citation
Furnace Atmospheres, Practical Heat Treating: Processes and Practices, By Jon L. Dossett, ASM International, 2024, p 39–59, https://doi.org/10.31399/asm.tb.phtpp.t59380039
Download citation file:
Related Book Content
Preface
Practical Heat Treating: Processes and Practices
About the Author
Practical Heat Treating: Processes and Practices
Glossary of Practical Heat Treating Terms
Practical Heat Treating: Processes and Practices
Types of Heat Treating Furnaces
Practical Heat Treating: Processes and Practices
Post-Processing of Additively Manufactured Metal Parts
Additive Manufacturing Processes
Fabrication of Wrought Stainless Steels
Metals Handbook Desk Edition (2nd Edition)
Process Control Considerations in Heat Treating
Metals Handbook Desk Edition (2nd Edition)
Heat Treating of Stainless Steels and Heat-Resistant Alloys
Metals Handbook Desk Edition (2nd Edition)
Heat Treating of Nonferrous Alloys
Metals Handbook Desk Edition (2nd Edition)