Chapter 6: Iron and Steel Melting Furnaces Available to Purchase
-
Published:2023
Page range:
115 - 144
Abstract
The melting furnace is a critically important piece of equipment in a foundry; it influences the balance between the metal required by molding machines and the melting capacity. This chapter presents the features, types, advantages, and applications of furnaces suitable for iron and steels such as cupolas, induction furnaces, and arc furnaces.
You do not currently have access to this chapter.
Citation
Iron and Steel Melting Furnaces, Casting Equipment Engineering Guide, By Jagan Nath, ASM International, 2023, p 115–144, https://doi.org/10.31399/asm.tb.ceeg.t59370115
Download citation file:
Related Book Content
Cast Iron Melting Furnaces
Cast Iron Science and Technology
Operation of Induction Furnaces in Iron Foundries
Induction Heating and Heat Treatment
Induction Glass Melting and Forming
Induction Heating and Heat Treatment
Steel Ingot Casting
Casting
Inert Gas Fusion
Materials Characterization
Machinery and Equipment for Direct and Indirect Hot Extrusion
Extrusion (Second Edition)
Induction Heating in Optical Fiber Draw Processing
Induction Heating and Heat Treatment
Horizontal Centrifugal Casting
Casting
Induction Furnaces
Casting
Electric Arc Furnace Melting
Casting