Iron and steel castings require cleaning as they come out of the shakeout units to remove any burned sand and sand that may remain stuck from the mold. This chapter presents the casting cleaning operation sequence. The sequence includes shot blasting; decoring or removal of cores from castings; degating or removal of runners, gates, and feeders; and flash removal and automation. The chapter also presents the objectives of heat treatment and discusses its processes. The chapter describes product quality control. Quality checks are grouped into three categories: material checks, product checks, and functional checks.