This chapter focuses on the elements and functions of sand conditioning equipment which are critical to achieving good quality castings. The sand conditioning equipment include sand muller; core sand mixers; sand conveyors and bucket elevators; sand aerators; mold conveyors; shakeout units; magnetic separators; lump breakers and core crushers; screens; sand coolers; sand reclamation systems; and sand hoppers.