Sand and metallic charge materials are two essential and heavy raw materials that are needed for molding and casting. This chapter focuses on planning and provision for storage and handling of the raw materials needed for casting manufacturing. The major raw materials used for molding and casting are metallic charge materials and nonmetallic materials. The chapter also presents the advantages, limitations, and applications of drum or rotary dryers (also known as rotary kiln dryers) and fluidized bed dryers (also known as vibration fluidized bed dryers).