Chapter 1: Casting Manufacturing Layout—Principles and Guidelines
-
Published:2023
Abstract
Planning and laying out casting facilities involve a number of vital factors, such as available infrastructure, selection of suitable sites, orientation of operations and process flow, markets and products, operating parameters, and targeted hourly output and annual capacity. This chapter presents guiding principles and layout concepts with these factors in mind. It also presents steps for the creation of a plant layout. Plant layout involves the arrangement of processing areas, machinery, and equipment for the efficient conversion of raw materials into finished products. The chapter discusses general guidelines for developing a layout.
Casting Manufacturing Layout—Principles and Guidelines, Casting Equipment Engineering Guide, By Jagan Nath, ASM International, 2023, p 1–12, https://doi.org/10.31399/asm.tb.ceeg.t59370001