Chapter 12: Aluminum in Light Vehicles Available to Purchase
-
Published:2023
Abstract
This chapter describes the different aluminum products used to manufacture modern automobile components. It discusses how automakers use these products to reduce weight, improve performance, and manage production costs. It also reflects on the changes in the aluminum industry, automakers, and their relationships. Organized by product type—castings, sheet, and extrusions—each section of the chapter describes the relevant alloys, tempers, and properties required to meet specific needs for component parts and final assembly.
Aluminum in Light Vehicles, Aluminum: Technology, Industry, and Applications, By Robert E. Sanders, Graeme J. Marshall, ASM International, 2023, p 265–302, https://doi.org/10.31399/asm.tb.atia.t59340265