Chapter 1: Introduction—Aluminum as an Industrial Material
-
Published:2023
Page range:
1 - 18
Abstract
This introduction presents an overview of the discovery of aluminum, the origins of the aluminum industry, and the evolution of the industry.
Topics
Aluminum
You do not currently have access to this chapter.
Citation
Introduction—Aluminum as an Industrial Material, Aluminum: Technology, Industry, and Applications, By Robert E. Sanders, Graeme J. Marshall, ASM International, 2023, p 1–18, https://doi.org/10.31399/asm.tb.atia.t59340001
Download citation file:
Related Book Content
Gallery of Aluminum Applications
Aluminum: Technology, Industry, and Applications
Preface
Aluminum: Technology, Industry, and Applications
About the Authors
Aluminum: Technology, Industry, and Applications
Effects of Metallurgical Variables on the Corrosion of Aluminum Alloys
Corrosion in the Petrochemical Industry (Second Edition)
Laser Stir Welding
Aluminum Science and Technology
Aluminum—The Light Metal
The History of Metals in America
Summary of Aluminum Temper Designations
Aluminum Science and Technology
Laser Beam Machining of Aluminum and Aluminum Alloys
Aluminum Science and Technology
Chemical and Electrolytic Brightening
Aluminum Science and Technology
Understanding the Corrosion Behavior of Aluminum
Corrosion of Aluminum and Aluminum Alloys