Abstract
This chapter describes the processes involved in heat treatment of carbon and low alloy steel, high strength low alloy steels, austenitic manganese steels, martensitic stainless steels, and austenitic stainless steels. In addition, precipitation hardening and quench hardening of carbon steel is also covered.
You do not currently have access to this chapter.
Citation
Hardenability and Heat Treatment, Steel Castings Handbook, 6th ed., Edited By Malcolm Blair, Thomas L. Stevens, ASM International, 1995, p 24-1–24-42, https://doi.org/10.31399/asm.tb.sch6.t68200327
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
Dissimilar Welds With Stainless Steels
Welding, Brazing, and Soldering
Compositions of Standard Carbon H-Steels and Standard Carbon Boron H-Steels
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Stainless Steels
Metallography of Steels Interpretation of Structure and the Effects of Processing
Stainless Steels
Alloying Understanding the Basics
Stainless Steels
Metallurgy for the Non-Metallurgist (Second Edition)
Heat Treatment of Stainless Steels
Practical Heat Treating Basic Principles
Austenitic Manganese Steels
Alloying Understanding the Basics
Heat Treating of Copper and Copper Alloys
Heat Treating of Nonferrous Alloys
Weldability and Welding
Steel Castings Handbook (Sixth Edition)
Properties of Stainless Steel Welds
Weld Integrity and Performance