Chapter 22: Heat-Resistant High Alloy Steels
-
Published:1995
Abstract
This chapter provides a detailed discussion on the definitions, alloy classification, alloy selection, mechanical properties, hot gas corrosion resistance, and formability of heat-resistant high alloy steels. In addition, the applications of cast heat-resistant alloys are also discussed.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Heat-Resistant High Alloy Steels, Steel Castings Handbook, 6th ed., Edited By Malcolm Blair, Thomas L. Stevens, ASM International, 1995, p 22-1–22-13, https://doi.org/10.31399/asm.tb.sch6.t68200298
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
6022 Automotive Sheet Alloy
Properties and Selection of Aluminum Alloys
Dual-Phase Steels
Advanced-High Strength Steels Science, Technology, and Applications
Complex-Phase Steels
Advanced-High Strength Steels Science, Technology, and Applications
Twinning-Induced Plasticity Steels
Advanced-High Strength Steels Science, Technology, and Applications
Austenitic Stainless Steels
Advanced-High Strength Steels Science, Technology, and Applications
6063 Extrusion Alloy
Properties and Selection of Aluminum Alloys
Selection and Application of Magnesium and Magnesium Alloys
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Forming of Refractory Metals
Metalworking: Sheet Forming
Forging and Forming
Superalloys: A Technical Guide (Second Edition)
Tube Hydroforming
Sheet Metal Forming Processes and Applications