Abstract
This chapter provides the definitions of fundamental wear mechanisms. The chapter describes the properties and applications of materials used for wear resistance. It discusses the processes involved in screening tests for wear resistance. In addition, the practical application of wear-resistant principles is covered.
You do not currently have access to this chapter.
Citation
Wear-Resistant Steels, Steel Castings Handbook, 6th ed., Edited By Malcolm Blair, Thomas L. Stevens, ASM International, 1995, p 19-1–19-21, https://doi.org/10.31399/asm.tb.sch6.t68200253
Download citation file:
Sept. 30 – Oct. 4 | Cleveland, Ohio
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2024 & IFHTSE World Congress!
Related Book Content
Introduction to Steel Castings
Steel Castings Handbook (Sixth Edition)
Industrial Applications of Steel Castings
Steel Castings Handbook (Sixth Edition)
Purchasing Policy
Steel Castings Handbook (Sixth Edition)
Casting Alloys
Stainless Steels for Design Engineers
Advantages of Steel Castings
Steel Castings Handbook (Sixth Edition)
Quality Control and Quality Assurance
Steel Castings Handbook (Sixth Edition)
Cast-Weld Construction
Steel Castings Handbook (Sixth Edition)
Finishing, Heat Treatment and Inspection
Steel Castings Handbook (Sixth Edition)
Process Capability and Tolerances
Steel Castings Handbook (Sixth Edition)