The design stresses for most pressure-containing structural application, which are based upon minimum mechanical properties designated in the specifications published by the American Society for Testing and Materials (ASTM). This chapter reviews metallurgical characteristics and their influence on the properties and performance of structural carbon and low alloy steels and contains a summary of the relevant features of the ASTM product specifications.