Abstract
This chapter provides an overview of the types of melting furnaces and refractories for steel casting. It then presents information about arc furnace melting and induction melting cycles. The chapter also describes methods for the removal of phosphorous, the removal of sulfur, and the recovery of elements from slag. It then presents an overview of argon-oxygen-decarburization (AOD) refining and types of ladles. The chapter describes chemical analysis that is performed using either optical emission or x-ray spectrographs.
You do not currently have access to this chapter.
Citation
Melting, Steel Castings Handbook, 6th ed., Edited By Malcolm Blair, Thomas L. Stevens, ASM International, 1995, p 14-1–14-10, https://doi.org/10.31399/asm.tb.sch6.t68200187
Download citation file:
Related Book Content
Melting and Melt Treatment of Aluminum Alloys
Aluminum Science and Technology
Computational Analysis of the Vacuum Arc Remelting (VAR) and Electroslag Remelting (ESR) Processes
Metals Process Simulation
Corrosion Failures of Industrial Refractories and Technical Ceramics
Corrosion: Materials
Modern Alloy Production
Metallurgy for the Non-Metallurgist (Second Edition)
Shape Casting of Steel
Casting
Magnesium and Magnesium Alloys
Casting
Introduction to Steel Castings
Steel Castings Handbook (Sixth Edition)
Industrial Applications of Steel Castings
Steel Castings Handbook (Sixth Edition)
Purchasing Policy
Steel Castings Handbook (Sixth Edition)
Casting Alloys
Stainless Steels for Design Engineers