Abstract
This chapter discusses the following conventional molding processes for static casting: green sand molding, dry sand molding, vacuum molding, and expendable pattern casting. It also discusses core and mold processes for steel castings. The chapter provides an overview of sand molds for large steel castings and a special sand molding process. It describes the following precision processes for static casting: investment casting, ceramic molding, and centrifugal casting.
You do not currently have access to this chapter.
Citation
Casting and Molding Processes, Steel Castings Handbook, 6th ed., Edited By Malcolm Blair, Thomas L. Stevens, ASM International, 1995, p 13-1–13-14, https://doi.org/10.31399/asm.tb.sch6.t68200173
Download citation file:
Related Book Content
Molding Methods
Metals Handbook Desk Edition (2nd Edition)
Overview of Casting Processes
Aluminum Castings Engineering Guide
Centrifugal Casting
Casting
No-Bond Sand Molding
Casting
Magnesium and Magnesium Alloys
Casting
Investment Casting
Superalloys: A Technical Guide (Second Edition)
Aluminum Shape Casting
Casting
Introduction to Steel Castings
Steel Castings Handbook (Sixth Edition)
Industrial Applications of Steel Castings
Steel Castings Handbook (Sixth Edition)