This chapter discusses the following conventional molding processes for static casting: green sand molding, dry sand molding, vacuum molding, and expendable pattern casting. It also discusses core and mold processes for steel castings. The chapter provides an overview of sand molds for large steel castings and a special sand molding process. It describes the following precision processes for static casting: investment casting, ceramic molding, and centrifugal casting.