Steel Castings Handbook (Sixth Edition)Available to Purchase
Steel Castings Handbook, Sixth Edition contains information and engineering data relevant to the design, manufacture, and application of steel castings. The book's content is organized into five multiple-chapter sections, covering the design process, manufacturing equipment and procedures, purchasing, detailed application examples, and material selection for property optimization and manufacturability. The handbook also includes an appendix with composition and hardness data for a wide range of casting alloys and coverage on heat treatments, molding methods, redesign for casting, and the effect of quality on component performance. With its detailed explanations and extensive use of illustrations, the book serves equally well as a reference, text, or guide for both new and experienced engineers. For information on the print version, ISBN 978-0-87170-556-3, follow this link.
Download citation file:
Table of Contents
-
Part 1: General Information
-
Chapter 2: Industrial Applications of Steel CastingsPublished:01 December 1995
-
Part 2: Purchasing Castings
-
Part 3: Designing Castings
-
Chapter 9: Engineering Drawings for Casting ProductionPublished:01 December 1995
-
Part 4: Manufacture of Castings
-
Chapter 15: Finishing, Heat Treatment and InspectionPublished:01 December 1995
-
Chapter 17: Quality Control and Quality AssurancePublished:01 December 1995
-
Part 5A: Material Selection - Mechanical and Chemical Properties
-
Chapter 20: Corrosion-Resistant High Alloy SteelsPublished:01 December 1995
-
Chapter 23: Low-Temperature and Cryogenic SteelsPublished:01 December 1995
-
Part 5B: Material Selection - Processing Properties
-
Part 5C: Material Selection - Physical Properties
-
Reference Information