Chapter 13: Hot-Work Tool Steels
-
Published:1998
Page range:
219 - 250
Abstract
Steels for hot-work applications, designated as group H steels in the AISI classification system, have the capacity to resist softening during long or repeated exposures to high temperatures needed to hot work or die cast other materials. These steels are subdivided into three classes according to the alloying approach: chromium hot-work steels, tungsten hot-work steels, and molybdenum hot-work steels. This chapter discusses the composition, characteristics, applications, advantages, and disadvantages of each of these steels.
You do not currently have access to this chapter.
Citation
Hot-Work Tool Steels, Tool Steels, 5th ed., By George Roberts, George Krauss, Richard Kennedy, ASM International, 1998, p 219–250, https://doi.org/10.31399/asm.tb.ts5.t65900219
Download citation file:
Related Book Content
Additive Manufacturing of Tungsten, Molybdenum, and Cemented Carbides
Additive Manufacturing Processes
Properties of Refractory Metal Welds
Weld Integrity and Performance
Properties and Selection of Powder Metallurgy Refractory Metals
Powder Metallurgy
Refractory Metal Alloys
Alloying Understanding the Basics
Special Metallurgical Welding Considerations for Refractory Metals
Welding, Brazing, and Soldering
Refractory Metals
Elements of Metallurgy and Engineering Alloys
Fully Dense Processing of Refractory Metal Powders
Powder Metallurgy
Powder Metallurgy Electrical Contact Materials
Powder Metallurgy
Forging of Refractory Metals
Metalworking: Bulk Forming
Forming of Refractory Metals
Metalworking: Sheet Forming