Chapter 12: High-Carbon, High-Chromium, Cold-Work Tool Steels Available to Purchase
-
Published:1998
Page range:
203 - 217
Abstract
The high-carbon, high-chromium tool steels, designated as group D steels in the AISI classification system, are the most highly alloyed cold-work steels. This chapter describes the microstructures and hardenability of high-carbon, high-chromium tool steels and discusses the processes involved in the hardening and tempering of tool steels. It also covers the selection criteria and applications of high-carbon, high-chromium tool steels.
You do not currently have access to this chapter.
Citation
High-Carbon, High-Chromium, Cold-Work Tool Steels, Tool Steels, 5th ed., By George Roberts, George Krauss, Richard Kennedy, ASM International, 1998, p 203–217, https://doi.org/10.31399/asm.tb.ts5.t65900203
Download citation file:
Related Book Content
Water-Hardening Tool Steels
Tool Steels (Fifth Edition)
Air-Hardening, Cold-Work Tool Steels
Tool Steels (Fifth Edition)
Oil-Hardening Cold-Work Tool Steels
Tool Steels (Fifth Edition)
Iron and Steel
Elementary Materials Science
Heating and Holding Times
Steel Heat Treating Technologies
Temper Colors for Steels
Heat Treating of Irons and Steels
Acoustical Characterization
Steel Heat Treating Technologies
Heat Treatment of High-Alloy Nickel-Cobalt Steels
Heat Treating of Irons and Steels
High Speed Steels
Tool Steels (Fifth Edition)
Mold Steels
Tool Steels (Fifth Edition)