Chapter 9: Thermodynamics of Microstructure Change Available to Purchase
-
Published:2008
Page range:
259 - 285
Abstract
This chapter provides a classification of the types of microstructural changes and transformations and then reviews each type. It presents the Johnson-Mehl-Avrami-Kolmogorov (JMAK) equation and explains the thermodynamics of eutectic solidification and eutectoid transformation. An appendix covers growth of eutectoid structure in carburized pearlite.
You do not currently have access to this chapter.
Citation
Thermodynamics of Microstructure Change, Thermodynamics of Microstructures, By Taiji Nishizawa, ASM International, 2008, p 259–285, https://doi.org/10.31399/asm.tb.tm.t52320259
Download citation file:
Related Book Content
Pearlite, Ferrite, and Cementite
Steels: Processing, Structure, and Performance (Second Edition)
Thermodynamics in Extrusion
Aluminum Extrusion Technology
Solid-State Transformations
Phase Diagrams Understanding the Basics
Thermal Expansion
Materials at Low Temperatures
Carburization and Metal Dusting
High-Temperature Corrosion and Materials Applications
Twinning-Induced Plasticity Steels
Advanced High-Strength Steels: Science, Technology, and Applications, Second Edition
Thermodynamics of Extraction
Beryllium Chemistry and Processing
Electrochemical Thermodynamics: The Gibbs Function, Electrochemical Reactions, and Equilibrium Potentials
Fundamentals of Electrochemical Corrosion
Microstructures and Characterization of Gray Irons
Cast Iron Science and Technology
Invariant Transformation Structures
Metallography and Microstructures