Chapter 3: Thermodynamics of Solutions
-
Published:2008
Abstract
This chapter explains the idea of solution theory and the nature of mixed materials. The chapter considers approximation of free energy by the regular solution model and sublattice model. It discusses chemical potential and nonrandom distribution based on the interactions between solute atoms.
You do not currently have access to this chapter.
Citation
Thermodynamics of Solutions, Thermodynamics of Microstructures, By Taiji Nishizawa, ASM International, 2008, p 55–89, https://doi.org/10.31399/asm.tb.tm.t52320055
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Introduction to Phase Transformations
Elements of Metallurgy and Engineering Alloys
Thermodynamics and Phase Diagrams
Phase Diagrams Understanding the Basics
Free Energy of Pure Substances
Thermodynamics of Microstructures
Solid Solutions and Phase Transformations
Alloy Phase Diagrams
Thermodynamics of Gaseous Corrosion
Corrosion: Fundamentals, Testing, and Protection
Principles of Aqueous Corrosion
Corrosion: Understanding the Basics