Abstract
Ductile iron has far superior mechanical properties compared to gray iron as well as significantly improved castability and attractive cost savings compared to cast steel. This chapter begins with information on graphite morphology and matrix type. It then discusses the advantages and applications of ductile iron. Next, the effects of various factors on the grades, chemistry, matrix, and mechanical properties of ductile iron are covered. This is followed by a section detailing the ductile iron treatment methods and the quality control methods used. Guidelines for gating and feeder design are then provided. Further, the chapter addresses the technology of...
Sign in
ASM members
Member Sign InEngineering Ductile Iron Castings, Iron and Steel Castings Engineering Guide, By Jagan Nath, ASM International, 2022, p 163–194, https://doi.org/10.31399/asm.tb.isceg.t59320163
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!