Ductile iron has far superior mechanical properties compared to gray iron as well as significantly improved castability and attractive cost savings compared to cast steel. This chapter begins with information on graphite morphology and matrix type. It then discusses the advantages and applications of ductile iron. Next, the effects of various factors on the grades, chemistry, matrix, and mechanical properties of ductile iron are covered. This is followed by a section detailing the ductile iron treatment methods and the quality control methods used. Guidelines for gating and feeder design are then provided. Further, the chapter addresses the technology of ductile iron castings, including the performance and geometric attributes, molding and core-making processes used, material grades, mechanical properties, and chemical compositions of a few applications. Finally, it describes ductile iron casting defects and presents practical cases of problem-solving.

You do not currently have access to this chapter.
Don't already have an account? Register
Close Modal

or Create an Account

Close Modal
Close Modal