This chapter describes the making of iconic structures such as the Chrysler Building. It also describes the discoveries of the Nirosta (18-8) stainless steel that was used for the construction of the Chrysler Building. The chapter presents William Van Alen's description of 18-8 stainless steel for the Chrysler Building. It provides information on the opening ceremonies for the Chrysler Building, Van Alen's vision, and the exterior of the building.