Abstract
This chapter examines the early literature on stainless steel to gain an understanding of the state-of-the-art of stainless steel as it progressed through the first 37 years after the discoveries made in Sheffield and Essen.
Topics
Stainless steel
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
The Early Books and Papers on Stainless Steel (1917–1949), The History of Stainless Steel, By Harold M. Cobb, ASM International, 2010, p 59–99, https://doi.org/10.31399/asm.tb.hss.t52790059
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
The Life of Harry Brearley (1871–1948)
The History of Stainless Steel
The Chrysler Building (1930) The Miracle on 42nd Street
The History of Stainless Steel
The Gateway Arch
The History of Stainless Steel
Stainless Steel Bibliography
The History of Stainless Steel
A Stainless Steel Timeline
The History of Stainless Steel
Pulp-and-Paper Industry Applications
Stainless Steels for Design Engineers
Introduction
The History of Stainless Steel
Canada Restores a Fleet of Stainless Steel Railcars
The History of Stainless Steel
The Plummer Classification System of Trade Names
The History of Stainless Steel
Glossary of Foundry Terms
Steel Castings Handbook (Sixth Edition)