Chapter 5: The Life of Harry Brearley (1871–1948)[1]
-
Published:2010
Page range:
33 - 57
Abstract
This chapter provides insights into the work of a stainless steel pioneer, Harry Brearley. It explains how Brearley's early life and experience led him to become a self-trained chemist and metallurgist.
Topics
Stainless steel
You do not currently have access to this chapter.
Citation
The Life of Harry Brearley (1871–1948), The History of Stainless Steel, By Harold M. Cobb, ASM International, 2010, p 33–57, https://doi.org/10.31399/asm.tb.hss.t52790033
Download citation file:
Related Book Content
The Early Books and Papers on Stainless Steel (1917–1949)
The History of Stainless Steel
The Chrysler Building (1930) The Miracle on 42nd Street
The History of Stainless Steel
The Gateway Arch
The History of Stainless Steel
Stainless Steel Bibliography
The History of Stainless Steel
A Stainless Steel Timeline
The History of Stainless Steel
The Accidental Birth of a No-Name Alloy
Metallurgy for the Non-Metallurgist (Second Edition)
Pulp-and-Paper Industry Applications
Stainless Steels for Design Engineers
Introduction
The History of Stainless Steel
Canada Restores a Fleet of Stainless Steel Railcars
The History of Stainless Steel
The Plummer Classification System of Trade Names
The History of Stainless Steel