Book Chapter
Appendix 13: Comparison of Hardness Tests
-
Published:1996
Page range:
432
Abstract
This appendix presents a comparison of hardness tests on indenters for different loads along with the applications of these tests.
Topics
Hardness testing
You do not currently have access to this chapter.
Citation
Comparison of Hardness Tests, Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels, By Charlie R. Brooks, ASM International, 1996, p 432, https://doi.org/10.31399/asm.tb.phtpclas.t64560432
Download citation file:
Sept. 30 – Oct. 4 | Cleveland, Ohio
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2024 & IFHTSE World Congress!
Related Book Content
Mechanical Properties
Steel Metallurgy for the Non-Metallurgist
Process Verification and Quality Assurance
Practical Heat Treating: Processes and Practices
Mechanical Testing and Properties of Plastics: An Introduction
Characterization and Failure Analysis of Plastics
Selection and Industrial Applications of Hardness Tests
Mechanical Testing and Evaluation