Appendix 7: Compositions of Standard Carbon Steels
-
Published:1996
Page range:
412
Abstract
This appendix contains tables listing the compositions of standard nonresulfurized carbon (1.0 manganese maximum and over 1.0 manganese) and the compositions of standard resulfurized and rephosphorized carbon steels.
You do not currently have access to this chapter.
Citation
Compositions of Standard Carbon Steels, Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels, By Charlie R. Brooks, ASM International, 1996, p 412, https://doi.org/10.31399/asm.tb.phtpclas.t64560412
Download citation file:
Sept. 30 – Oct. 4 | Cleveland, Ohio
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2024 & IFHTSE World Congress!
Related Book Content
Compositions of Standard Carbon H-Steels and Standard Carbon Boron H-Steels
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Steel Cross Reference
Heat Treating of Irons and Steels
Stress-Corrosion Cracking of Carbon and Low-Alloy Steels (Yield Strengths Less Than 1241 MPa)
Stress-Corrosion Cracking: Materials Performance and Evaluation (Second Edition)
Hydrogen Damage in a Waterwall Boiler Tube Section
Handbook of Case Histories in Failure Analysis
Austenitizing Temperatures for Steels
Failure Analysis of Heat Treated Steel Components
Hardenability Curves
Properties and Selection: Irons, Steels, and High-Performance Alloys
Excavator Boom Lift Equalizer Hose Failure
ASM Failure Analysis Case Histories: Construction, Mining, and Agricultural Equipment
Hardness Conversions
Steels: Processing, Structure, and Performance (Second Edition)
AISI to Non-AISI Steel Cross Reference
Failure Analysis of Heat Treated Steel Components
Summary of Fusion Welding Processes
Welding Fundamentals and Processes