Appendix 2: Common Units for Converting from the English to the Metric (SI) System
-
Published:1996
Page range:
404
Abstract
This data sheet includes a select list of factors for converting customary English units to metric (SI) units.
You do not currently have access to this chapter.
Citation
Common Units for Converting from the English to the Metric (SI) System, Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels, By Charlie R. Brooks, ASM International, 1996, p 404, https://doi.org/10.31399/asm.tb.phtpclas.t64560404
Download citation file:
Sept. 30 – Oct. 4 | Cleveland, Ohio
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2024 & IFHTSE World Congress!
Related Book Content
Metric Stress or Pressure Conversions
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Typical Room-Temperature Physical Properties of Wrought Aluminum Alloys
Properties and Selection of Aluminum Alloys