Appendix 1a: ASTM Standard A255-89 Method for Calculating Hardenability from Composition Available to Purchase
-
Published:1996
Page range:
389 - 401
Abstract
This chapter discusses the method for calculating hardenability from composition. It contains tables listing multiplying factors, carbon content, initial hardness, and 50% martensite hardness. The tables also list Jominy distance for 50% martensite vs. DI (in. and mm), boron factors vs. % carbon and alloy factor, and distance hardness dividing factors for non-boron and boron steels (in. and mm).
You do not currently have access to this chapter.
Citation
ASTM Standard A255-89 Method for Calculating Hardenability from Composition, Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels, By Charlie R. Brooks, ASM International, 1996, p 389–401, https://doi.org/10.31399/asm.tb.phtpclas.t64560389
Download citation file:
Related Book Content
Hardenability Bands of Alloy Steels
Heat Treating of Irons and Steels
Heat Treating of Cold-Work Tool Steels—Medium-Alloy Air-Hardening, High-Carbon High-Chromium and High-Vanadium-Powder Metallurgy Steels
Heat Treating of Irons and Steels
Hardenability Calculation of Carbon and Low-Alloy Steels with Low or Medium Carbon
Steel Heat Treating Fundamentals and Processes
Decarburization
Carburizing Microstructures and Properties
Sources of Failures in Carburized and Carbonitrided Components
Failure Analysis of Heat Treated Steel Components
Boost/Diffuse Cycles for Carburizing
Practical Heat Treating (Second Edition)
Steels in the Annealed and Normalized Conditions
Light Microscopy of Carbon Steels
Carburizing
Gear Materials, Properties, and Manufacture
Pack Carburizing
Steel Heat Treating Fundamentals and Processes
Dual-Phase Steels
Properties and Selection: Irons, Steels, and High-Performance Alloys