Chapter 8: Structural Steels
-
Published:1996
Abstract
Structural steels are used for components such as I-beams and automobile frames. This chapter focuses on processing these steels to attain a fine primary ferrite grain size to develop high strength. It first reviews the concepts and principles of recrystallization in plastically deformed metals. The chapter reviews the concepts of annealing of cold worked metals. It then looks at hot working and the grain size associated with it. Additionally, the chapter reviews the methods of strengthening in the steels that rely mainly on reduction in the primary ferrite grain size. It discusses basic methods used to develop a small austenite grain size, and hence a small primary ferrite grain size. Then, the chapter covers the processes involved in the precipitation hardening of the ferrite. Finally, it examines some commercial thermomechanical processes used on structural steels, namely hot deformation and controlled cooling.
Structural Steels, Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels, By Charlie R. Brooks, ASM International, 1996, p 263–306, https://doi.org/10.31399/asm.tb.phtpclas.t64560263
Download citation file:
Sept. 30 – Oct. 4 | Cleveland, Ohio
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2024 & IFHTSE World Congress!