Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Chapter 2: The Iron-Carbon Phase Diagram and Time-Temperature-Transformation (TTT) Diagrams
-
Published:1996
Abstract
This chapter describes the two types of Time-Temperature-Transformation (TTT) diagrams used and outlines the methods of determining them. As a precursor to the examination of the decomposition of austenite, it first reviews the phases and microconstituents found in steels. This includes a presentation of the iron-carbon phase diagram and the equilibrium phases. The chapter also covers the common microconstituents that form in steels, including the nomenclature used to describe them. The chapter provides a comparison of isothermal and continuous cooling TTT diagrams. These diagrams are affected by the carbon and alloy content and by the prior austenite grain size,...
Sign in
ASM members
Member Sign InThe Iron-Carbon Phase Diagram and Time-Temperature-Transformation (TTT) Diagrams, Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels, By Charlie R. Brooks, ASM International, 1996, p 3–41, https://doi.org/10.31399/asm.tb.phtpclas.t64560003
Download citation file:
2022 ASM International Catalog: Issue 1
View new, upcoming, and best-selling ASM Handbooks, technical books, and databases.