Book Chapter
Reference Tables Available to Purchase
-
Published:2004
Page range:
273 - 277
Abstract
This chapter contains tables listing room-temperature tensile yield strength comparisons of metals and plastics and room-temperature tensile modulus of elasticity comparisons of various materials.
You do not currently have access to this chapter.
Citation
Reference Tables, Tensile Testing, 2nd ed., Edited By J.R. Davis, ASM International, 2004, p 273–277, https://doi.org/10.31399/asm.tb.tt2.t51060273
Download citation file:
Related Book Content
Glossary of Terms: Mechanical Testing and Evaluation
Mechanical Testing and Evaluation
Aluminum Structural Design
Properties and Selection of Aluminum Alloys
Corrosion Rate Conversion
Corrosion: Environments and Industries
Corrosion Rate Conversion
Corrosion: Fundamentals, Testing, and Protection
Description of Hardness Code and Specification of Hardness Numbers for Metals
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Etchants for Revealing Macrostructure
Metallography Principles and Practice
Attack Polishing Procedures
Metallography Principles and Practice
Chemical Polishing Solutions
Metallography Principles and Practice
Plastic Design Methods
Characterization and Failure Analysis of Plastics
Viscoelasticity of Plastics
Characterization and Failure Analysis of Plastics