Book Chapter
Chapter 15: High Strain Rate Tensile Testing
-
Published:2004
Page range:
251 - 263
Abstract
High strain rate tensile testing is used to understand the response of materials to dynamic loading. The behavior of materials under high strain rate tensile loads may differ considerably from that observed in conventional tensile tests. This chapter discusses the processes involved in determining strain rate effects in tension by conventional tensile tests and covers expanding ring tests, flat plate impact tests, split-Hopkinson pressure bar tests, and rotating wheel tests.
You do not currently have access to this chapter.
Citation
High Strain Rate Tensile Testing, Tensile Testing, 2nd ed., Edited By J.R. Davis, ASM International, 2004, p 251–263, https://doi.org/10.31399/asm.tb.tt2.t51060251
Download citation file:
Related Book Content
Glossary of Terms
Tensile Testing (Second Edition)
Tensile Testing of Elastomers
Tensile Testing (Second Edition)
Introduction to High Strain Rate Testing
Mechanical Testing and Evaluation
Tensile Testing of Plastics
Tensile Testing (Second Edition)
Tensile Testing of Ceramics and Ceramic-Matrix Composites
Tensile Testing (Second Edition)
Testing and Inspection of Metals—The Quest for Quality
Metallurgy for the Non-Metallurgist (Second Edition)
Introduction to Tensile Testing
Tensile Testing (Second Edition)
Tensile Testing for Determining Sheet Formability
Tensile Testing (Second Edition)
Tensile Testing at Low Temperatures
Tensile Testing (Second Edition)
Tensile Testing for Design
Tensile Testing (Second Edition)