Book Chapter
Chapter 8: Tensile Testing of Plastics Available to Purchase
-
Published:2004
Page range:
137 - 153
Abstract
The testing of plastics includes a wide variety of chemical, thermal, and mechanical tests. This chapter reviews the tensile testing of plastics, which has been standardized in ASTM D 638, "Standard Test Method for Tensile Properties of Plastics," and other comparable standards. It describes the fundamental factors that affect data from tensile tests, examines the stipulations in standardized tensile testing, and discusses the utilization of data from tensile tests.
You do not currently have access to this chapter.
Citation
Tensile Testing of Plastics, Tensile Testing, 2nd ed., Edited By J.R. Davis, ASM International, 2004, p 137–153, https://doi.org/10.31399/asm.tb.tt2.t51060137
Download citation file:
Related Book Content
Glossary of Terms
Tensile Testing (Second Edition)
Tensile Testing of Elastomers
Tensile Testing (Second Edition)
Tensile Testing of Ceramics and Ceramic-Matrix Composites
Tensile Testing (Second Edition)
High Strain Rate Tensile Testing
Tensile Testing (Second Edition)
Plastic Design Methods
Characterization and Failure Analysis of Plastics
Viscoelasticity of Plastics
Characterization and Failure Analysis of Plastics
Ultrasonic Nondestructive Analysis of Plastics
Characterization and Failure Analysis of Plastics
Glossary of Terms—Characterization and Failure Analysis of Plastics
Characterization and Failure Analysis of Plastics
Abbreviations—Characterization and Failure Analysis of Plastics
Characterization and Failure Analysis of Plastics
Environmental Stress Cracking
Characterization and Failure Analysis of Plastics