Abstract
This chapter first lists the compositions of typical steels that are suitable for nitriding. It then presents considerations for steel selection. The chapter also shows the influence of alloying elements on hardness after nitriding and the depth of nitriding. It provides a detailed discussion on plasma nitriding of type 422 stainless steel, nitriding of type 440A and type 630 (17-4 PH) stainless steel. The chapter also discusses plasma nitride case depths.
Sign in
ASM members
Member Sign InSteels For Nitriding, Practical Nitriding and Ferritic Nitrocarburizing, By David Pye, ASM International, 2003, p 125–138, https://doi.org/10.31399/asm.tb.pnfn.t65900125
Download citation file:
Understanding the Basics Collection
8-Volume Digital Library Exclusive
The Understanding the Basics Collection provides comprehensive coverage of critical topics in metallurgy. These introductory guides present critical information on key topics related to materials processing, performance, and evaluation.