Chapter 10: Nitriding in Fluidized Beds
-
Published:2003
Abstract
A fluidized-bed furnace system can be used for the gas nitriding process. This chapter focuses on fluidized-bed nitriding. It discusses the methods of heating a fluidized bed. The heating system can be electrical or gas, and internal or external. The chapter describes nitriding and oxynitriding processes in the fluidized-bed furnace. It also explains how to operate the fluid bed for nitriding. The chapter provides a discussion on the measurement of the gas dissociation.
Sign in
ASM members
Member Sign InNitriding in Fluidized Beds, Practical Nitriding and Ferritic Nitrocarburizing, By David Pye, ASM International, 2003, p 111–118, https://doi.org/10.31399/asm.tb.pnfn.t65900111
Download citation file:
Understanding the Basics Collection
8-Volume Digital Library Exclusive
The Understanding the Basics Collection provides comprehensive coverage of critical topics in metallurgy. These introductory guides present critical information on key topics related to materials processing, performance, and evaluation.