This chapter discusses the processes involved in the wetting, spreading, and chemical interaction of a braze on a nonmetal. The chapter reviews the key materials and process issues relating to the joining of nonmetals using active brazing. Emphasis is placed on the differences in brazing to metals by established methods. The chapter also describes the designing process and properties of metal/nonmetal joints.