Optical Microscopy of Fiber-Reinforced CompositesAvailable to Purchase
ASM International
ISBN electronic:
978-1-62708-349-2
Publication date:
2010
Book Chapter
Chapter 12: Matrix Microstructural Analysis Available to Purchase
-
Published:2010
Page range:
211 - 222
Abstract
Microstructural analysis of the composite matrix is necessary to understand the performance of the part and its long-term durability. This chapter focuses on the microstructural analysis of engineering thermoplastic-matrix composites and the influence of cooling rate and nucleation on the formation of spherulites in high-temperature thermoplastic-matrix carbon-fiber-reinforced composites. It also describes the microstructural analysis of a bio-based thermosetting-matrix natural fiber composite system.
You do not currently have access to this chapter.
Citation
Matrix Microstructural Analysis, Optical Microscopy of Fiber-Reinforced Composites, By Brian S. Hayes, Luther M. Gammon, ASM International, 2010, p 211–222, https://doi.org/10.31399/asm.tb.omfrc.t53030211
Download citation file:
Related Book Content
Matrix Microstructure Analysis of Fiber-Reinforced Composites
Metallography and Microstructures
Impact Response of Composites
Optical Microscopy of Fiber-Reinforced Composites
Failure of a Fuel Nozzle in an Aircraft Engine
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of a Low-Pressure Turbine Rotor (LPTR) Blade
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of Center Support Bearings in an Aircraft Engine
Failure Analysis of Engineering Structures Methodology and Case Histories
Environmental Performance of Concrete
Corrosion: Materials
Failure of a Turbine Blade in an Aircraft Engine
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of Shutter Bolts in a Reaction Control Valve in an Aircraft
Failure Analysis of Engineering Structures Methodology and Case Histories
Quantitative Microscopy
Metallography Principles and Practice