Chapter 10: Toughening Methods for Thermoset-Matrix Composites
-
Published:2010
Abstract
The second-generation composite materials were added to increase the strain to failure of the primary phase and/or create a dispersed second phase, thereby enhancing the fracture toughness of the thermosetting matrix. These matrices offered novel design capabilities for composites in a variety of aircraft applications. To improve the damage tolerance of composite materials even further, an engineering approach to toughening was used to modify the highly stressed interlayer with either a tougher material or through the use of preformed particles, leading to the third generation of composite materials. This chapter discusses the development, processes, application, advantages, and disadvantages of...
Sign in
ASM members
Member Sign InToughening Methods for Thermoset-Matrix Composites, Optical Microscopy of Fiber-Reinforced Composites, By Brian S. Hayes, Luther M. Gammon, ASM International, 2010, p 177–191, https://doi.org/10.31399/asm.tb.omfrc.t53030177
Download citation file:
Understanding the Basics Collection
8-Volume Digital Library Exclusive
The Understanding the Basics Collection provides comprehensive coverage of critical topics in metallurgy. These introductory guides present critical information on key topics related to materials processing, performance, and evaluation.