Book Chapter
Chapter 6: Casting, Forming, and Forging
-
Published:2005
Page range:
129 - 137
Abstract
Gear manufacture depends on machinery available, design specifications or requirements, cost of production, and type of material from which the gear is to be made. This chapter discusses the processes involved in methods for manufacturing gears, namely casting, forming, and forging.
You do not currently have access to this chapter.
Citation
Casting, Forming, and Forging, Gear Materials, Properties, and Manufacture, Edited By J.R. Davis, ASM International, 2005, p 129–137, https://doi.org/10.31399/asm.tb.gmpm.t51250129
Download citation file:
Related Book Content
Forging and Forming
Titanium: A Technical Guide (Second Edition)
Forging and Forming
Superalloys: A Technical Guide (Second Edition)
Fabrication of Wrought Stainless Steels
Metals Handbook Desk Edition (2nd Edition)
Fabrication and Finishing of Metal Products
Metallurgy for the Non-Metallurgist (Second Edition)
Metalworking
Beryllium Chemistry and Processing
Titanium
Elements of Metallurgy and Engineering Alloys
Processing of Titanium and Titanium Alloys
Metals Handbook Desk Edition (2nd Edition)
Forging of Discontinuously Reinforced Aluminum Composites
Metalworking: Bulk Forming
Principles of Forging Machines
Cold and Hot Forging Fundamentals and Applications