Fatigue and Durability of Metals at High Temperatures
Chapter 9: Obstacles to High-Temperature Structural Durability of Continuous-Fiber Metal-Matrix Composites
-
Published:2009
Abstract
Fiber-reinforced metal-matrix composites have carved out a niche in applications requiring high strength to weight ratios, but they are susceptible to failure when exposed to high temperatures and cyclic loads. This chapter discusses the obstacles that must be overcome to improve the creep-fatigue behavior of these otherwise promising materials. It addresses six areas that have been the focus of intense research, including thermal-expansion and elastic-viscoplastic mismatch, thermally induced biaxiality and interply stresses, creep and cyclic relaxation of residual stresses, and enhanced interfaces for oxidation.
Sign in
ASM members
Member Sign InObstacles to High-Temperature Structural Durability of Continuous-Fiber Metal-Matrix Composites, Fatigue and Durability of Metals at High Temperatures, By S.S. Manson, G.R. Halford, ASM International, 2009, p 223–230, https://doi.org/10.31399/asm.tb.fdmht.t52060223
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.