Fatigue and Durability of Metals at High Temperatures
Chapter 8: Critique of Predictive Methods for Treatment of Time-Dependent Metal Fatigue at High Temperatures
-
Published:2009
Abstract
This chapter provides a detailed review of creep-fatigue analysis techniques, including the 10% rule, strain-range partitioning, several variants of the frequency-modified life equation, damage assessment based on tensile hysteresis energy, the OCTF (oxidation, creep, and thermomechanical fatigue) damage model, and numerous methods that make use of creep-rupture, crack-growth, and void-growth data. It also discusses the use of continuum damage mechanics and includes examples demonstrating the accuracy of each method as well as the procedures involved.
Sign in
ASM members
Member Sign InCritique of Predictive Methods for Treatment of Time-Dependent Metal Fatigue at High Temperatures, Fatigue and Durability of Metals at High Temperatures, By S.S. Manson, G.R. Halford, ASM International, 2009, p 173–221, https://doi.org/10.31399/asm.tb.fdmht.t52060173
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.