Abstract
Increasing the efficiency of power plants by operating at higher temperatures and pressures and adding a double-reheat feature comes at the expense of shortened lifetimes for critical components. This chapter provides an overview of the material-related problems associated with advanced steam plants and their respective solutions. The discussion covers the selection of materials on a component-specific basis for boilers as well as steam turbines.
You do not currently have access to this chapter.
Citation
Materials for Advanced Steam Plants, Damage Mechanisms and Life Assessment of High-Temperature Components, By R. Viswanathan, ASM International, 1989, p 383–413, https://doi.org/10.31399/asm.tb.dmlahtc.t60490383
Download citation file:
Related Book Content
The Materials Selection Process
Metallurgy for the Non-Metallurgist (Second Edition)
Modeling of Diffusion Bonding
Metals Process Simulation
Erosion and Erosion-Corrosion
High-Temperature Corrosion and Materials Applications
Selection and Weldability of Non-Heat-Treatable Aluminum Alloys
Welding, Brazing, and Soldering
Introduction to the Effects of Composition, Processing, and Structure on Materials Properties
Materials Selection and Design
Introduction and Overview of Design Considerations and Materials Selection
Metals Handbook Desk Edition (2nd Edition)
Selection of Superalloys
Superalloys: A Technical Guide (Second Edition)
Selection of Heat Treat Process for Optimum Gear Design
Heat Treatment of Gears A Practical Guide for Engineers
Navigating the Plastic Material Selection Process
Characterization and Failure Analysis of Plastics
Corrosive Wear Failures
Failure Analysis and Prevention (2021 Edition)