Increasing the efficiency of power plants by operating at higher temperatures and pressures and adding a double-reheat feature comes at the expense of shortened lifetimes for critical components. This chapter provides an overview of the material-related problems associated with advanced steam plants and their respective solutions. The discussion covers the selection of materials on a component-specific basis for boilers as well as steam turbines.