Abstract
This appendix contains drawings that illustrate the test specimens used in generating the data related to aluminum alloy castings.
Topics
Microstructure,
Casting defects,
Rotating bend fatigue testing,
Corrosion-resistant alloys,
High-temperature alloys,
Cast aluminum alloys,
Aluminum alloys,
Expendable mold casting,
Filling and feeding,
Permanent mold casting,
Aging,
Annealing,
Quenching,
Solution heat treatment,
Alloy composition,
Creep properties,
Fatigue properties,
Fracture toughness,
Brinell hardness,
Stress-strain curves,
Tensile properties,
Viscoelastic properties,
Physical properties,
Thermal expansion,
Mechanical testing,
Cast metal products,
Measuring and testing instruments
You do not currently have access to this chapter.
Citation
Test Specimen Drawings, Aluminum Alloy Castings: Properties, Processes, and Applications, By J. Gilbert Kaufman, Elwin L. Rooy, ASM International, 2004, p 301–304, https://doi.org/10.31399/asm.tb.aacppa.t51140301
Download citation file:
Related Book Content
Glossary of Terms
Aluminum Alloy Castings Properties, Processes, and Applications
Abbreviations and Symbols
Aluminum Alloy Castings Properties, Processes, and Applications
Nominal Compositions and Composition Limits for Aluminum Alloy Castings
Properties and Selection of Aluminum Alloys
Fracture Resistance of Aluminum Alloys
Properties and Selection of Aluminum Alloys
Aluminum Casting Processes
Aluminum Alloy Castings Properties, Processes, and Applications
Static Mechanical Tests for Filament-Wound Composites
Composite Filament Winding
Fatigue and Fracture Properties of Aluminum Alloy Castings
Fatigue and Fracture
Aluminum Foundry Products
Metals Handbook Desk Edition (2nd Edition)
The Effects of Microstructure on Properties
Aluminum Alloy Castings Properties, Processes, and Applications